Brazing joins parts by heating them to more than 840°F and applying a filler metal that has a melting temperature below that of the base metal. Filler metal flows into the joint by capillary ...
SAE Transactions, Vol. 104, Section 6: JOURNAL OF PASSENGER CARS: Part 1 (1995), pp. 266-272 (7 pages) Kaiser Aluminum & Chemical Corporation, in cooperation with Ravenswood Aluminum Corporation, ...
The joining of magnesium and titanium alloys represents a vital area of materials science, given the need for high-performance, lightweight structures in aerospace, automotive and other advanced ...